How to produce refractory bricks:
First, the stones are ground, then they are turned into soft soil, and after 3 days of baking in the furnace, they are baked at a temperature above 1500 degrees Celsius. This.
Of course, this brick with its high thermal resistance is widely used in furnaces, pans and industrial insulation. But its normal type is used with some changes in the facades of buildings.